Rust yellow heavy place can use paper towel posted once, prolong the reaction time. If the effect not beautiful, can repeat. 2. HB - X102 in shandong white linen sometimes does have some light red granite, it is recommended to use diluted with water. As for use 1:1 existing residual, reoccupy some pigment scavenging agents processing.
Because of shandong white linen contain iron minerals in water is easy to produce overmuch, generating pitting oxidation reaction. Water, is one of the key factors to produce rusty spot.
So when, face-lifting to prevent pitting can from the following several aspects to consider:
1. Refurbished must be used before filling plugging all crevices glue;
2. With "green before face-lifting angel" G713 strong permeability alkali type oily protectants (green marble second generation product) deep protection, shandong white linen deep into 5 ~ 10mm, face-lifting depth about in commonly 2mm or so. So can effectively guarantee the construction water won't enter granite internal;
3. When renovation, reduce water timely bibulous the retention time;
4. Don't make mirror surface wet process.